Abstract

A thermodynamic approach has been used to progress in the understanding of the chemical processes taking place in the casting furnaces. The ceramic mould materials used for the casting of superalloys vaporize at high temperature under vacuum and the vapors condense then in the colder zones of the furnace. In addition, the graphite of the furnace resistor perturbs the vaporization regime of the moulds and is at the origin of other vaporization and condensation processes. The deposition regime of impurities leading to inclusions formation during the casting of the metal is modified. The thermodynamic analysis is confirmed by observations made on the superalloy casting furnaces. The deposits observed and characterized correspond to those predicted by the thermodynamic analysis, but the mass losses of the moulds producing these deposits are 60 times smaller than predicted.

Information

Type
Research Article
Copyright
© La Revue de Métallurgie, 2003

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable