Finite element analysis of residual stress and interlayer in hard coating/interlayer/soft substrate system during nanoindentation

Published online by Cambridge University Press:  31 January 2011

Liuhe Li*
Affiliation:
School of Physics and Materials Science, City University of Hong Kong, Kowloon, Hong Kong, People’s Republic of China; and School of Mechanical Engineering and Automation, Beijing University of Aeronautics and Astronautics, Beijing 100083, China
Lan Yin
Affiliation:
School of Physics and Materials Science, City University of Hong Kong, Kowloon, Hong Kong, People’s Republic of China; and School of Mechanical Engineering and Automation, Beijing University of Aeronautics and Astronautics, Beijing 100083, China
Paul K. Chu*
Affiliation:
School of Physics and Materials Science, City University of Hong Kong, Kowloon, Hong Kong, People’s Republic of China
Get access

Abstract

The mechanical properties of thin films are frequently evaluated using nanoindentation. The finite element method (FEM) is very effective for investigating the stress and strain fields of the film–substrate system during nanoindentation. However, the role of residual stress and the thin interlayer between the film and substrate is not well known, especially when the hard coating/interlayer/soft substrate are considered together. In this work, the FEM is used to investigate the load-displacement behavior of the hardness of the hard coating/interlayer/soft substrate system. The load–displacement process is simulated, and the effects of different residual stresses and interlayer thicknesses are discussed.

Information

Type
Articles
Copyright
Copyright © Materials Research Society 2008

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

REFERENCES

1Oliver, W.C.Pharr, G.M.: An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments. J. Mater. Res. 7, 1564 1992CrossRefGoogle Scholar
2Ma, D.Xu, K.: Numerical simulation for determining the mechanical properties of thin metal films using depth-sensing indentation technique. Thin Solid Films 323, 183 1998CrossRefGoogle Scholar
3Zheng, Z.W.Sridhar, I.: Spherical indentation of an elastic thin film on an elastic-ideally plastic substrate. Mater. Sci. Eng., A 423, 64 2006CrossRefGoogle Scholar
4Gan, L.Ben-Nissan, B.: The effects of mechanical properties of thin films on nano-indentation data: Finite element analysis. Comput. Mater. Sci. 8, 273 1997CrossRefGoogle Scholar
5Sampath, K., Vanimisetti, R.Narasimhan, R.: A numerical analysis of spherical indentation response of thin hard films on soft substrates. Int. J. Solids Struct. 43, 6180 2006Google Scholar
6Souza, R.M., Mustoe, G.G.W.Moore, J.J.: Finite element modeling of the stresses, fracture and delamination during the indentation of hard elastic films on elastic–plastic soft substrates. Thin Solid Films 356, 303 1999CrossRefGoogle Scholar
7Souza, R.M., Mustoe, G.G.W.Moore, J.J.: Numerical and experimental study of the circular cracks observed at the contact edges of the indentations of coated systems with soft substrates. Thin Solid Films 392, 65 2001CrossRefGoogle Scholar
8Sriram, K., Narasimhan, R.Biswas, S.K.: A numerical fracture analysis of indentation into thin hard films on soft substrates. Eng. Fract. Mech. 70, 1323 2003CrossRefGoogle Scholar
9Lichinchi, M., Lenardi, C., Haupt, J.Vitali, R.: Simulation of Berkovich nanoindentation experiments on thin films using finite element method. Thin Solid Films 312, 240 1998CrossRefGoogle Scholar
10Bennani, H. HoumidTakadoum, J.: Finite element model of elastic stresses in thin coatings submitted to applied forces. Surf. Coat. Technol. 111, 80 1999CrossRefGoogle Scholar
11D’Haen, J., Quaeyhaegens, C., Stals, L.M.Van Stappen, M.: Interface study of physical vapour deposition TiN coatings on plasma-nitrided steels. Surf. Coat. Technol. 61, 194 1993CrossRefGoogle Scholar
12Zhou, L.Tian, J.: Analysis and experimental validation of residue stress of the coated cutting tools. New Technol. New Proc. 5, 81 2007 in ChineseGoogle Scholar
13Swadener, J.G., Taljat, B.Pharr, G.M.: Measurement of residual stress by load and depth-sensing indentation with spherical indenters. J. Mater. Res. 16(7), 2091 2001CrossRefGoogle Scholar
14Olivas, E.R., Swadener, J.G.Shen, Y.L.: Nanoindentation measurement of surface residual stresses in particle-reinforced metal matrix composites. Scripta Mater. 54(2), 263 2006CrossRefGoogle Scholar
15Bolshakov, A., Oliver, W.C.Pharr, G.M.: Influences of stress on the measurement of mechanical properties using nanoindentation: Part II. Finite element simulations. J. Mater. Res. 11(3), 760 1996CrossRefGoogle Scholar
16Suresh, S.Giannakopoulos, A.E.: A new method for estimating residual stresses by instrumented sharp indentation. Acta Mater. 46(16), 5755 1998CrossRefGoogle Scholar
17Chechenin, N.G., Bøttiger, J.Krog, J.P.: Nanoindentation of amorphous aluminum oxide films II: Critical parameters for the breakthrough and a membrane effect in thin hard films on soft substrates. Thin Solid Films 261(1–2), 228 1995CrossRefGoogle Scholar
18Carlsson, S.Larsson, P.L.: On the determination of residual stress and strain fields by sharp indentation testing: Part I. Theoretical and numerical analysis. Acta Mater. 49(12), 2179 2001CrossRefGoogle Scholar
19Pelletier, H., Krier, J.Mille, P.: Characterization of mechanical properties of thin films using nanoindentation test. Mech. Mater. 38, 1182 2006CrossRefGoogle Scholar
20Bressan, J.D., Tramontin, A.Rosa, C.: Modeling of nanoindentation of bulk and thin film by finite element method. Wear 258, 115 2005CrossRefGoogle Scholar
21Sridhar, I.Zheng, Z.W.: Effect of friction and adhesion on the load-displacement of a spherical probe in contact with a compliant incompressible elastic coating. Tribol. Int. 40, 180 2007CrossRefGoogle Scholar
22ASM International ASM Handbook of Metal Materials vol. 3, 3rd ed.ASM Warrendale, PA 1991 27Google Scholar
23Pischow, K.A., Eriksson, L., Harju, E.Korhonen, A.S.: The influence of titanium interlayers on the adhesion of PVD TiN coatings on oxidized stainless steel substrates. Surf. Coat. Technol. 58, 163 1993CrossRefGoogle Scholar