X-Ray Fractography on Fatigue Fracture Surfaces of Mg-9mass%Al-1mass%Zn Alloy

Published online by Cambridge University Press:  06 March 2019

Yoichi Kishi
Affiliation:
Material Research and Testing Center, Nippon Institute of Technology 4-1 Gakuendai, Miyashiro-machi, Saitama 345, Japan
Get access

Extract

X-ray diffraction observation of fracture surfaces provides fracture analysis with useful information on the mechanisms and mechanical conditions of fracturing. This method is called ” X-ray fractography “ and has been developed especially in Japan as a new engineering tool for fracture analysis.

In the present paper, X-ray fractography is applied to fatigue fracture surfaces of AZ91 magnesium alloy which are used for machine parts. The X-ray stress constant, H,was first determined. The fatigue tests were conducted by using compact tension ( CT ) specimens of AZ91 magnesium alloy. The residual stress was measured on and beneath the fatigue fracture surface. The depth of the plastic zone left on the fatigue fracture surface was evaluated from the residual stress distribution. The results are discussed on the basis of fracture mechanics.

Information

Type
Research Article
Copyright
Copyright © International Centre for Diffraction Data 1995

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

[1] Hirose, Y., Yajima, Z. and Mura, T., “X-Ray Fractography on Fatigue Fracture Surfaces of AISI 4340 Steel”, Advances in X-Ray Analysis, Vol. 29, 63;1986.Google Scholar
[2] Kishi, Y., Yajima, Z. and Hirose, Y., “X-Ray Fractography of Light Metals”, Proceedings of the Conference of Advanced Technology in Experimental Mechanic., 361, 1993. .Google Scholar
[3] Annual Book of ASTM Standards, Vol. 03. 01, E647-91, 654: 1991.Google Scholar
[4] Kishi, Y., Hirose, Y., Satoh, T., Ninomiya, R. and Kubota, K., “X-Ray Fractography on Fatigue Fracture Surfaces of ZAS Alloy”, Advances in Electronic Packaging, Vol. 2, 791; 1992.Google Scholar
[5] Levy, N., Marcal, P. V., Ostengren, W. J. and Rice, J. R., “Small Scale Yielding Near a Crack in Plane Strain: A Finite Element Method”, International Journal of Fracture Mechanics, Vol. 7, 143;1971.Google Scholar
[6] Tanaka, K. and Hatanaka, N., “X-Ray Fractography of Fatigue Fracture of Steels”, Vol. 33, 324:1984.Google Scholar